| An example of the surface roughness pattern that
develops on the surface of the off-critical dPEP/PEP mixtures as a
result of two-dimensional spinodal decomposition in the sub-surface
layer that is depleted in dPEP due to its segregation to the vacuum
surface. The lateral dimensions on the scanning force micrograph
are in micrometers. |